Superior printing quality with sharper images, more open intermediate depths, finer highlight dots and less dot gain, i.e. larger range of tonal values therefore improved contrast and produce flat top dots when adequate process equipment are used
High resilience and good resistance towards mechanical impacts deliver excellent durability
Increased productivity and data transfer without loss of quality due to digital workflow
Excellent ink transfer using water and alcohol-based inks
Cost effective and more environmentally friendly in processing, as no film is required
Suitable for corrugated post printing and other paper substrates
Thickness (mm/inch) | Hardness (Shore Å) | Total Range(%) | Screen Ruling(LPI) | Minimum Isolated Line | Minimum Isolated Dot |
2.84/0.112 | 42 | 2 ‒ 95% | 120 | 0.1mm | 0.2mm |
3.18/0.125 | 41 | 2 ‒ 95% | 120 | 0.2mm | 0.5mm |
3.94/0.155 | 37 | 2 ‒ 95% | 100 | 0.3mm | 0.75mm |
4.70/0.185 | 35 | 3 ‒ 95% | 80 | 0.3mm | 0.75mm |
6.35/0.250 | 35 | 3 ‒ 95% | 80 | 0.3mm | 0.75mm |
Thickness (mm/inch) | Back Exposure (s) | Main Exposure (mins) | Wash out (mm/mins) | Drying Time (h) | Post Exposure (mins) | Detack(mins) |
2.84/0.112 | 50-80 | 10-15 | 120-140 | 2-2.5 | 5min | 4min |
3.18/0.125 | 80-110 | 10-15 | 100-130 | 2.5-3 | 5min | 4min |
3.94/0.155 | 90-120 | 10-15 | 100-130 | 3 | 5min | 4min |
4.70/0.185 | 150-200 | 10-15 | 70-100 | 3 | 5min | 4min |
6.35/0.250 | 250-300 | 10-15 | 50-90 | 3 | 5min | 4min |
*Run-Length varies with its printing conditions and imaging content